What is the Storage Stability of Ammonium Metatungstate Dispersions at High or Low Temperatures?

The storage stability of ammonium metatungstate dispersions at high or low temperatures can be affected by a variety of factors, including the temperature itself, the concentration of the dispersion, the pH value, the presence of other additives, and the material of the storage container, etc. The following is an analysis of the storage stability of ammonium metatungstate dispersions at different temperatures. The following is an analysis of the storage stability of ammonium metatungstate dispersions under different temperature environments:

 

  1. Storage stability under high temperature environment

Under high temperature environment, the stability of ammonium metatungstate dispersion may be affected by the following:

Acceleration of chemical reaction

High temperature will accelerate the thermal movement between molecules, which may lead to the acceleration of chemical reaction between ammonium metatungstate molecules and other components, thus affecting the stability of dispersion.

Volatilization and evaporation

Under high temperature environment, the solvent (e.g. water) in the dispersion may accelerate volatilization and evaporation, leading to an increase in the concentration of the dispersion, which in turn may affect its stability and use.

Particle aggregation

High temperatures may lead to increased particle movement in the dispersion, increasing the chance of particle collisions, which may promote particle aggregation and precipitation.

 

Therefore, when storing ammonium metatungstate dispersions under high temperature environment, it is necessary to take appropriate measures to maintain its stability, such as controlling the storage temperature, using storage containers with good sealing, avoiding direct sunlight and so on.

 

Storage stability under low temperature environment

The stability of ammonium metatungstate dispersion under low temperature environment may also be affected to some extent, but its influence may be smaller compared with high temperature environment:

 

Change of solubility

Although the solubility of ammonium metatungstate is temperature-dependent, its solubility usually does not change much at low temperatures, so it is unlikely to lead to a large amount of precipitation of particles.

 

Crystallization precipitation

However, if the temperature is too low, the solvent in the dispersion may freeze or form ice crystals, which may lead to crystallization and precipitation of solutes in the dispersion (e.g., ammonium metatungstate), thus affecting its homogeneity and stability.

 

Frozen containers

If storage containers are not made of materials suitable for low temperatures, they may freeze and crack or deform, leading to leakage or contamination of the dispersion.

 

Therefore, when storing ammonium metatungstate dispersion in low-temperature environment, it is also necessary to pay attention to choosing suitable storage containers and storage conditions, such as avoiding extreme low temperature and using low-temperature resistant storage containers.

 

The storage stability of ammonium metatungstate dispersion in high or low temperature environment will be affected to some extent. In order to ensure its stability and use effect, it is necessary to choose suitable storage conditions and measures according to the specific situation. At the same time, in the process of storage and use, it is also necessary to pay attention to regular inspection of the state and performance changes of the dispersing liquid, so as to take timely measures to adjust and deal with.

More details of ammonium metatungstate product, please visit website: http://ammonium-metatungstate.com/
Please contact CHINATUNGSTEN for inquiry and order of ammonium metatungstate:
Email: sales@chinatungsten.com
Tel.: 86 592 5129595

0